The EB 24 Film Creep Tester from ELASTOCON is designed based on the EB 10-II ageing
oven. This instrument has a digital ruler system which includes a laser line pointer
to measure the creep manually. The ruler is also connected to a computer that will
transfer the values into a spreadsheet template and the results/graphs will be
calculated automatically.
The oven perform well according to the apparatus requirements in ISO 188, IEC 811
and other equivalent standards.