Stress relaxation tests are very effective for conducting ageing tests, as substantial amounts of information result with little effort, especially when using the continuous measurement system.

Stress relaxation tests are becoming more and more popular for determination of rubber properties. From the beginning stress relaxation tests were used mainly in scientific projects at universities, but a growing use has been shown in recent years. This may be caused by the introduction of stress relaxation tests in product standards, such as sealing rings for pipes. The automotive industry has also started to specify stress relaxation tests for critical sealing products in the cars.

Manufacturer website: http://www.elastocon.se