Materials Testing > Thermal and Rheological Properties > Thermal Analysis

Differential Scanning Calorimeter (DSC)

(Available in: Thailand, Indonesia and Vietnam)

Differential Scanning Calorimeter (DSC) is the method to measure energetic effect in solid and liquid under controlled temperature changes. The typical features of DSC are analysis of glass transition temperature (Tg), melting/crystallization behavior, specific heat (Cp), oxidative stability, O.I.T., and etc.

Facts and Advantages (*depending on model):
  • 3D heating furnace
  • Constantan (CuNi) disk sensor with high thermal conductivity of silver carrier plate
  • Simultaneous connecting to LN2 and Intra-cooler cooling system
  • Able to couple with FTIR and MS
Temperature range-170 to 2,000°C
Measuring range+/- 600 mW
Signal time constant3 sec
Baseline drift<10µW
Pressure rangeVacuum up to 15 MPa